Figure 8
Low-temperature experiments. Samples were cooled in field-free space, then given a near-saturation remanence in an applied field of 800 mT at −170 °C and rewarmed in zero field to room temperature. A, Dolerite Dyke; B, Trachytic Dyke; C, Felsic Granodiorite; D, Quartz Diorite.